dc.description.abstractBitumen holds the aggregate in hot mix asphalt (HMA). Without asphalt binder, HMA would simply be crushed stone or gravel. A bitumen batching system (BBS) is comprised of bitumen storage, transportation, weighing and discharge equipment in an asphalt mixing plant (AMP). The function of the equipment is to batch the binder heated up to working temperature and to discharge it into a mixer in batches. In the entire system, the binder is exposed to high temperature and oxygen. Bitumen is slowly oxidized when it is in contact with oxygen. The degree of oxidation is highly dependent on temperature, time and thickness of a bitumen film. This article models the key factors influencing on the dynamics of bitumen oxidation in BBS equipment. Stone mastic asphalt (SMA) mixture was produced from the same materials according to the same job-mix formula (JMF) in neighbouring batch type AMP by changing the mixing time of materials from 20 to 60 s. Bitumen binder was separated from the taken SMA samples and its gradation was identified. Thus, Marshall specimens were produced and tested. Penetration Pen25 of bitumen binder recovered in rotary evaporator, softening point Tsp was determined and penetration index Ip was calculated. The presented findings of experimental investigation show that the properties of bitumen binder in BBS working at two different technologies changed inconsistently. Due to gravitation, the bitumen intensively flowing into a mixer (BBS1) is impacted by oxidation more than the bitumen batched by a high-pressure pump (BBS2).eng
dc.formatPDF
dc.format.extentp. 862-872
dc.format.mediumtekstas / txt
dc.language.isoeng
dc.relation.isreferencedbyScience Citation Index Expanded (Web of Science)
dc.relation.isreferencedbyScopus
dc.relation.isreferencedbyICONDA
dc.relation.isreferencedbyINSPEC
dc.source.urihttp://www.tandfonline.com/doi/pdf/10.3846/13923730.2013.843587
dc.titleDependences of SMA mixture and its bituminous binder properties on bitumen batching system, mixing time and temperature on asphalt mixing plant
dc.typeStraipsnis Web of Science DB / Article in Web of Science DB
dcterms.accessRightsIDS Number: 278BM
dcterms.references54
dc.type.pubtypeS1 - Straipsnis Web of Science DB / Web of Science DB article
dc.contributor.institutionVilniaus Gedimino technikos universitetas
dc.contributor.institutionUAB "Fegda"
dc.contributor.facultyTransporto inžinerijos fakultetas / Faculty of Transport Engineering
dc.subject.researchfieldT 002 - Statybos inžinerija / Construction and engineering
dc.subject.researchfieldT 003 - Transporto inžinerija / Transport engineering
dc.subject.enBitumen
dc.subject.enHot mix asphalt (HMA)
dc.subject.enStone mastic asphalt (SMA)
dc.subject.enBitumen batching system (BBS)
dc.subject.enJob-mix formula (JMF)
dc.subject.enOxidation, short-term ageing
dc.subject.enRheology
dc.subject.enPenetration
dc.subject.enViscosity
dc.subject.enAsphalt mixing plant (AMP)
dcterms.sourcetitleJournal of civil engineering and management
dc.description.issueno. 6
dc.description.volumeVol. 19
dc.publisher.nameTechnika
dc.publisher.cityVilnius
dc.identifier.doi000328863000008
dc.identifier.doi2-s2.0-84891352087
dc.identifier.doi10.3846/13923730.2013.843587
dc.identifier.elaba4055656


Šio įrašo failai

FailaiDydisFormatasPeržiūra

Su šiuo įrašu susijusių failų nėra.

Šis įrašas yra šioje (-se) kolekcijoje (-ose)

Rodyti trumpą aprašą