• Lietuvių
    • English
  • Lietuvių 
    • Lietuvių
    • English
  • Prisijungti
Peržiūrėti įrašą 
  •   DSpace pagrindinis
  • Mokslinės publikacijos (PDB) / Scientific publications (PDB)
  • Moksliniai ir apžvalginiai straipsniai / Research and Review Articles
  • Straipsniai Web of Science ir/ar Scopus referuojamuose leidiniuose / Articles in Web of Science and/or Scopus indexed sources
  • Peržiūrėti įrašą
  •   DSpace pagrindinis
  • Mokslinės publikacijos (PDB) / Scientific publications (PDB)
  • Moksliniai ir apžvalginiai straipsniai / Research and Review Articles
  • Straipsniai Web of Science ir/ar Scopus referuojamuose leidiniuose / Articles in Web of Science and/or Scopus indexed sources
  • Peržiūrėti įrašą
JavaScript is disabled for your browser. Some features of this site may not work without it.

Lowering cement content in mortar by adding superfine zeolite as cement replacement and optimizing mixture proportions

Thumbnail
Data
2019
Autorius
Chen, J.J.
NG, Pui Lam
Kwan, A.K.H.
Li, L.G.
Metaduomenys
Rodyti detalų aprašą
Santrauka
Reducing the cement consumption in concrete construction is an effective method to lower the carbon footprint and alleviate global warming. One strategy is to replace part of cement by a cementitious or non-cementitious filler. Another strategy is to optimize the mixture proportions to minimize the cement content. Although these strategies have been separately adopted, there is little research on their combined adoption. To study the feasibility of combining these two strategies, a number of mortar samples with varying amount of superfine zeolite (SZ) added, binder/aggregate (B/A) ratio and water/binder (W/B) ratio were made for packing density, flowability, cohesiveness and strength tests. The results revealed that adding 5% SZ to replace cement would increase the packing density and flowability and decrease the cement/strength ratio by 17%–28%, depending on the other mixture parameters. There is an optimum B/A ratio for minimum cement/strength ratio, which is generally lower at lower strength level. The use of a suitable B/A ratio of 0.65 or 0.55 instead of a constant and conservative value of 0.75 at strength level lower than 60 MPa could reduce the cement content by about 10%.
Paskelbimo data (metai)
2019
URI
https://etalpykla.vilniustech.lt/handle/123456789/125023
Kolekcijos
  • Straipsniai Web of Science ir/ar Scopus referuojamuose leidiniuose / Articles in Web of Science and/or Scopus indexed sources [7946]

 

 

Naršyti

Visame DSpaceRinkiniai ir kolekcijosPagal išleidimo datąAutoriaiAntraštėsTemos / Reikšminiai žodžiai InstitucijaFakultetasKatedra / institutasTipasŠaltinisLeidėjasTipas (PDB/ETD)Mokslo sritisStudijų kryptisVILNIUS TECH mokslinių tyrimų prioritetinės kryptys ir tematikosLietuvos sumanios specializacijosŠi kolekcijaPagal išleidimo datąAutoriaiAntraštėsTemos / Reikšminiai žodžiai InstitucijaFakultetasKatedra / institutasTipasŠaltinisLeidėjasTipas (PDB/ETD)Mokslo sritisStudijų kryptisVILNIUS TECH mokslinių tyrimų prioritetinės kryptys ir tematikosLietuvos sumanios specializacijos

Asmeninė paskyra

PrisijungtiRegistruotis